Energy-efficient production of thermoplastic starch
- research
Thermoplastic starch (TPS) represents a promising alternative to fossil-based polymeric materials due to its availability, biodegradability and renewable origin. However, optimising processing conditions and reducing the energy demands of production remain significant challenges for its wider industrial application. In this context, reducing the average molecular weight of native starch represents a potential strategy for improving its processability while maintaining suitable thermomechanical properties.
To this end, native wheat starch was modified by acid hydrolysis (AH) for different treatment durations (1, 2 and 4 hours) and subsequently converted into thermoplastic starch using a previously developed two-step protocol consisting of solution casting and melt mixing.
The AH-modified systems were compared with unmodified TPS and TPS containing 5 wt% maltodextrin (MD) as a viscosity-reducing additive. While acid hydrolysis reduces the average molecular weight through the scission of polymer chains, maltodextrin, as a starch oligomer, acts both as a low-molecular-weight component and as a lubricant fully compatible with the polymer matrix.
The materials were thoroughly characterised in terms of their morphology, mechanical, micromechanical and rheological properties, as well as their processing behaviour. Increasing the duration of acid hydrolysis treatment resulted in a moderate reduction in TPS homogeneity and a slight increase in crystallinity, leading to a modest increase in macro- and micromechanical stiffness.
The effect of acid hydrolysis on rheological properties was relatively limited due to the competing effects of reduced molecular weight in the amorphous phase and increased stiffness associated with the presence of crystalline domains.
The most significant finding concerns the reduction in processing torque and temperature, measured in situ during laboratory-scale sample preparation by melt mixing. Acid hydrolysis enabled TPS processing at a lower melt-mixing temperature (110 °C instead of 120 °C).
These results demonstrate that acid hydrolysis is an effective strategy for reducing the processing demands of thermoplastic starch while maintaining suitable thermomechanical properties, offering potential benefits in terms of energy efficiency in the production of starch-based materials.
Speaker
Miroslav Šlouf is Associate Professor and Head of the Department of Polymer Morphology at the Institute of Macromolecular Chemistry of the Czech Academy of Sciences in Prague.
He obtained his PhD from Charles University in Prague in 2001. His research focuses on polymer morphology, electron microscopy and diffraction, and the relationships between the structure and mechanical and micromechanical properties of polymers, with particular emphasis on biodegradable and biocompatible materials and their biomedical applications.
Author of more than 300 scientific publications and co-author of numerous scientific contributions and patents, he has extensive international teaching and research experience and has also served as a Visiting Professor at the University of Trento.